We measured the difference among the 2.0mm RP and 2.0mm SP in bending stiffness, bending strength, and bending structural stiffness. The hypothesis was as follows:

H1: There is a significant difference among the 2.0mm RP and 2.0mm SP in bending stiffness, bending strength, and bending structural stiffness.

We conducted ANOVA to test the hypothesis for this study. There was a significant difference among the 2.0mm RP and 2.0mm SP in bending stiffness, bending strength, and bending structural stiffness (p<0.05).